this post was submitted on 21 Apr 2024
45 points (97.9% liked)

3DPrinting

15590 readers
55 users here now

3DPrinting is a place where makers of all skill levels and walks of life can learn about and discuss 3D printing and development of 3D printed parts and devices.

The r/functionalprint community is now located at: !functionalprint@kbin.social or !functionalprint@fedia.io

There are CAD communities available at: !cad@lemmy.world or !freecad@lemmy.ml

Rules

If you need an easy way to host pictures, https://catbox.moe/ may be an option. Be ethical about what you post and donate if you are able or use this a lot. It is just an individual hosting content, not a company. The image embedding syntax for Lemmy is ![](URL)

Moderation policy: Light, mostly invisible

founded 1 year ago
MODERATORS
 

Anyone have any idea what might cause this sort of issue on PLA? I run into it frequently, but pretty much only when all of the following points are true:

  • the print has multiple parts, so the extruder spends a decent amount of time off of any given part (only one part from this print is pictured)
  • the affected part(s), like the picture above, have a relatively steep outward overhang, extending over the build plate
  • the outward overhang part is relatively narrow, as seen from a top view

This is from a printer with a 4028 fan (i.e. pretty massive airflow, server type fan) so even the 35-45% (based on layer time) I have it currently set at is more than 100% with single/dual 5015's or etc.

I guess my other option is to try supports, but this doesn't really seem like a situation where supports should be needed. Anyone ever had a similar problem and solved it without just turning the speed waaaayyyyyy down?

you are viewing a single comment's thread
view the rest of the comments
[–] mihnt@lemmy.ca 2 points 6 months ago

From my experience that glitter filament seems to absorb moisture a little faster than some filaments. I keep mine in a drybox all the time.