Thank you all for your help! After yesterday's Input I managed to Print my Box! The Problem was (mostly) the Bed temperature! The lower Bed temperature (60°C) and the now successful Firmware-Update (special thanks to DABDA) done the trick!

Thank you all for your help and your advice!

Hello I'm very new to 3D printing, I'm using a Sovol 06 with 1.75mm PLA. I'm trying to print a Box (for MTG-Cards). But everytime the bottom of the Box starts to "deatche" itself from the Bed. It starts with one corner and then progresses to the whole print. The Nozzle temperature is 200°C and the Bed temperature is 80°C. Can someone help?

you are viewing a single comment's thread
view the rest of the comments
[-] DABDA@lemmy.world 4 points 10 months ago

Are you saying the surface in the picture is the one that touches the bed? If that's the case it should be nearly perfectly flat and smooth(ish depending on bed texture). If that's the orientation it prints in there's still an issue of distance and possibly belt tension or something else because of those waves and deep grooves. There's a bunch of different methods to level a bed but ultimately you want the nozzle to slightly squish the filament it is putting down, in the picture it looks like it might not be.

As for the bed being clean, if you haven't yet I'd definitely spray some isopropyl alcohol and wipe it off, taking care not to touch the bed with your hands at all -- oil from your skin will easily cause adhesion issues.

Larger prints in general, and especially if there's temperature variance while printing (drafts), can start to pull off the bed as the material contracts. You may need to add a brim in your slicer to help keep it welded down. When it's necessary to use one will be a learning experience as you get used to your particular printer and environment.

[-] Roflmasterbigpimp@lemmy.world 2 points 10 months ago* (last edited 10 months ago)

Yes this is the Site in contact with the Bed. In my actual Try I've "loosend" the PLA a bit from the Coil so it can be passed down easier and decreased the printing speed. If that's fails I'm gonna try to clean it with alcohol. Thank you for the advice! :D

[-] GrindingGears@lemmy.ca 4 points 10 months ago

Drop your Z axis more than it was in the pic, I'd try at least two 0.05mm more steps down, and maybe even more. You want PLA to be pretty squashed. Stick a piece of computer paper in between the nozzle and the bed and lower the nozzle to the point that it takes a fair bit of resistance to pull the piece of paper out. That's the amount of z offset you want with PLA.

As others have said, you need to cool off a bit too, try 60 bed, 195 nozzle. See how it goes, you can always go up a bit or down a bit as it prints too. Try 60/195 though, no fan for the first 3 or 4 layers.

this post was submitted on 26 Nov 2023
32 points (100.0% liked)

3DPrinting

15330 readers
198 users here now

3DPrinting is a place where makers of all skill levels and walks of life can learn about and discuss 3D printing and development of 3D printed parts and devices.

The r/functionalprint community is now located at: !functionalprint@kbin.social or !functionalprint@fedia.io

There are CAD communities available at: !cad@lemmy.world or !freecad@lemmy.ml

Rules

If you need an easy way to host pictures, https://catbox.moe may be an option. Be ethical about what you post and donate if you are able or use this a lot. It is just an individual hosting content, not a company. The image embedding syntax for Lemmy is ![](URL)

Moderation policy: Light, mostly invisible

founded 1 year ago
MODERATORS