This does happen.
+1 for glue stick.
Also a layer of blue painters tape works well for me.
Another thing I've had good success with is cleaning the bed well with 95% IPA (thanks resin printing!) Then dropping the build plate with print attached into the freezer for a bit after it's done.
I used to do tape, but i really like the smooth finish that bare glass gives. Glue stick gave me bed adhesion issues, and i cant easily remove the glass bed.
I think the glass delaminated while it was cooling normally, not when i was prying it off.
You might look into a smooth build plate. It can take the damage and just be replaced.
I went with glass originally as it seemed at the time to be durable and therefore less waste. I don't want to generate extra waste. And those pei sheets dont look cheap :/